trammi
etching InGaAs/Inp?
trammi
2002-02-02
Hi,


I am trying to etch InGaAs/InP junction with HCL:CH3COOH:H2O2 (6:4:1) at temp 2
Deg. Centigrade. But i found that the surface is not uniform. and i'm unable to
standardize the etch rate of sample with the above solution. I need info
regarding this and related journals also.


Thanks in advance...


Krishna.






Get Your Private, Free E-mail from Indiatimes at  http://email.indiatimes.com
Buy Music, Video, CD-ROM, Audio-Books and Music Accessories from
http://www.planetm.co.in

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group