MEMSnet Home: MEMS-Talk: Various linewidths
Various linewidths
2002-02-04
Michael Roper
2002-02-05
Mighty Platypus
2002-02-06
Michael D Martin
Various linewidths
Michael Roper
2002-02-04
Hello all,

I am trying to etch glass using photolithography/wet etching techniques,
but I have made an observation during my lithography steps. I use a
photomask with various horizontal and vertical lines (all 5 um in width),
after exposing the photoresist (AZ1520) to UV light, developer, and
finally Cr etch, I have noticed that the horizontal lines are ~twice as
wide as the vertical lines.  Interestingly, by keeping the mask in the
same orientation to the glass, but moving the UV box 90 degrees, the
vertical lines then become ~twice as big as the horizontal lines.

I was wondering if this was a common occurence and if there is a simple
solution....thought about spinning the photomask and glass or the UV light
as the glass was being exposed, but just curious if there was a simpler
solution?  Thanks in advance to any help you can give.

Mike


Michael Roper
University of Florida
Chemistry Department
352-846-0838

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation