A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SU-8 bonding
SU-8 bonding
2002-02-05
Peng Jin
2002-02-05
Kevin Banks
SU-8 bonding
Peng Jin
2002-02-05
Hello everyone,

In my experiment, I need to bond the SU-8 parts with silicon or other
material. Could anyone give me some idea about it?

Thanks

>=========================================
>Dr. P. Jin
>Research Associate
>School of Manufacturing and Mechanical Engineering
>The University of Birmingham
>Edgbaston, Birmingham B15 2TT
>Tel:  ++44-121-414-4256
>=========================================

reply
Events