Au sticking on oxide & Dry etch simulation software
2002-02-06
Michael D Martin
Au sticking on oxide & Dry etch simulation software
Michael D Martin
2002-02-06
Hi Randall,
   I can help you out with 1, in order to get gold to stick without an
adhesion layer you need to do energetic ion deposition. There are
serveral companies that can help you out, one that comes to mind is
Skion Corp. in NJ. www.skion.com .

-Mike

>>> [email protected] 02/03/02 10:56PM >>>
Dear MEMS colleagues,

1) I am trying to get Au patterns adhere to either silicon
oxide or nitride or even silicon without any barriers /
adhesion layers. Any good tricks or solutions? Is lift-off
viable?

2) Any non-commercial software for me to download to
perform dry etching evaluation with different process
parameters? And can the software adopt a RIE, ICP, or ECR
mode form of etching?

Please kindly advise. Many thanks in advance.

Best,
Randall, Ph.D
Singapore,DLS
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Nano-Master, Inc.