It's actually low. 0.0035 micron/min at 85C

Best Regards,
Rafiqul Islam


EV Group Inc.- Technology- Tel: (602) 437 9492 x 118, (602)2842134
(cell),Fax: (602) 437 9435,
e-mail: [email protected] web: www.EVGroup.com


-----Original Message-----
From: Brian Semak [mailto:[email protected]]
Sent: Friday, February 08, 2002 6:13 AM
To: [email protected]
Subject: [mems-talk] Si (111) etch rates


I would like to know if anyone has done or know of some results of the etch
rate of 111 planes in silicon, in KOH. The values I've found in the
litterature seems to low.

Med venlig hilsen/Kind regards

Brian S. Semak, M.Sc. (Phys.)
R&D Hermetic Packaging

Hymite Aps
DTU, Bygn. 325, 1st floor
2800 Lyngby

Telephone(Direct): + 45 4525 9147
Fax:                     + 45 4525 9156
E-mail: [email protected]
www.hymite.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation