MEMSnet Home: MEMS-Talk: electroplating solder
porous alumina
2002-02-27
Shimin Xu
electroplating solder
2002-02-27
alexander li
2002-02-28
Steffan Intemann
electroplating solder
Steffan Intemann
2002-02-28
Try the solution from a german company called SCHLVTTER
(http://www.schloetter.de/english/chemie.htm)
We have used the SLOTOLET BP 10 for electroplating solder bumps for flip
chip applications.


Steffan Intemann

U-L-M photonics
Albert Einstein-Allee 45
D-89081 Ulm
Phone: +49(0)731/50260-40
Fax: +49(0)73150260-21
E-mail: [email protected]

www.ulm-photonics.de



-----Urspr|ngliche Nachricht-----
Von: [email protected] [mailto:[email protected]]Im
Auftrag von alexander li
Gesendet: Mittwoch, 27. Februar 2002 22:26
An: [email protected]
Betreff: [mems-talk] electroplating solder


Hi, there,

Does anyone know what is the solution to electroplate
pb/Sn solder, where can I buy it and what are the
device requirements of solder electroplating? Any
suggestions are greatly appreciated. Have a nice day!

Yours,
Alex
Yahoo! Greetings - Send FREE e-cards for every occasion!
http://greetings.yahoo.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review