black wax
2002-02-25
ABHIJAT GOYAL
2002-02-26
Maurice Norcott
2002-02-28
Dave Summers
2002-02-26
Karl Cazzini
2002-03-01
Roger Brennan
black wax
Dave Summers
2002-02-28
Hi,
Effective solvents for removing Apiezon. Black Wax are Xylene,Toluene (not
necessarily hot) and Chlorinated hydrocarbons such as Methylene Chloride and
Trichloroethylene.  Aliphatic hydrocarbons such as Hexane can also be used
but they are not as effective. The Wax is INSOLUBLE in  Ketones such as
Acetone and in Alcohols such as Ethanol and Iso Propanol.
Dave Summers
Technical Service Manager
Apiezon Products Ltd.
*********************************

----- Original Message -----
From: Maurice Norcott 
To: 
Sent: 26 February 2002 17:26
Subject: RE: [mems-talk] black wax


> Try Ted Pella or SPI, both electron microscopy supply houses. I think
> VWR may carry Apiezon black wax also. Acetone or hot toluene will remove
> the wax, followed with isopropyl rinse.
>
> -----Original Message-----
> From: ABHIJAT GOYAL [mailto:[email protected]]
> Sent: Monday, February 25, 2002 7:13 PM
> To: [email protected]
> Subject: [mems-talk] black wax
>
>
> Hi,
>
>  can you please suggest me some vendors for Black Wax as a mask for KOH
> etch.
> Can you please tell me the vendors that are based in US only, since it
will
> be
> difficult for me to procure my order if they are outside the US.
>
>   Also can you please suggest me something by which I can remove black wax
> after I have etched.
>
> Thanks in advance,
>
> Abhijat Goyal
>
>
> Abhijat Goyal
> EE MEMS group,
> MS candidate,
> Dept. Of Electrical Engineering,
> State College, PA
>
> Ph: (R)814-2350917
>     (O)814-8653664
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
>
> ________________________________________________________________________
> This e-mail has been scanned for all viruses by Star Internet. The
> service is powered by MessageLabs. For more information on a proactive
> anti-virus service working around the clock, around the globe, visit:
> http://www.star.net.uk
> ________________________________________________________________________
>


________________________________________________________________________
This e-mail has been scanned for all viruses by Star Internet. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group