silicon etching
1996-07-19
[email protected]
silicon etching
[email protected]
1996-07-19
We are etching deep pits (50-100
microns) into Si using acid (HF-HNO3-
CH3COOH) etch. There is no problem with bare silicon, but when the wafer
has a mask of Ti/Au then a strong texture develops on the etched surface.
This is likely due to an electrochemical process or to contamination
of the etching solution. Before switching over to KOH, does anyone have
any ideas on the cause of the texture and its cure??


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
The Branford Group
Tanner EDA by Mentor Graphics