Using AZ300 PR developer to etch Al
2002-03-13
Chan Ho Yin
Using AZ300 PR developer to etch Al
Chan Ho Yin
2002-03-13
Hi,


    According the suggestion from previuos post, I have tried to etch Al
using AZ300 developer. And using AZ5214 as a mask. I found that the pattern
is not good enough. Some of the pattern is etched by the developer. About
10%.  And all others are quite good.  What'w worng??  Can someone suggest
me how to mask my Al? Or what should I do to AZ5214 for a good protestion?

    Also, if I use ~1.6um AZ5214 to mask a layer (~2um) Al, is it possible
to etch Al thoroughly? Will the PR be etched competely before Al??

Thank You

Hoyin

_________________________________________________________________
MSN ,[C/4#(Q1z3LB23f*:$h&!$@(I(C&C&L1z*:,[$y!A=P2>&\
http://photos.msn.com/support/worldwide.aspx!C

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer