Regarding:  Glen Landry 
Subject: [mems-talk] SU-8 spinning problems

I had similar difficulties with SU-8.  One method that seemed to work for us was
to squeegee a thin layer of SU-8 across the entire substrate.  Then immediately
add more resist in the center, the usual amount, and spin.  A quick and dirty
solution, but it worked for us and kept my substrates from looking like spin
art.  Best of luck to you.

Dara Ruggiero
Harris Corporation

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.