MEMSnet Home: MEMS-Talk: single crystalline quartz micromachining
single crystalline quartz micromachining
2002-03-20
Gary Bernstein
2002-03-20
Jim Beall
single crystalline quartz micromachining
Gary Bernstein
2002-03-20
Hello,

Can anyone give me some basic references on the micromachining of
single crystalline quartz?  The closer to a tutorial on the materials
and basic processing the better.

Thanks very much,

Gary H. Bernstein
University of Notre Dame
[email protected]

______________________________________________________________
Gary H. Bernstein                       (219) 631-6269 (office)
Professor and Associate Chair           (219) 631-4393 (fax)
Department of Elec. Eng.                (219) 277-0752 (home)
275 Fitzpatrick Hall
University of Notre Dame
Notre Dame, IN  46556
[email protected]

See webpages at http://www.nd.edu/~micro/
                 http://www.nd.edu/~gbernste/
_______________________________________________________________

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing