Rifai, Sami
2002-03-25
Birol Kuyel
2002-03-25
[email protected]
2002-03-29
[email protected]
Etching
Birol Kuyel
2002-03-25
Dear Sami,

We manufacture custom PECVD, RIE, and Sputter Coaters. Please let us
know your requirements.

Best Regards,

Birol Kuyel, Ph.D.
NANO-MASTER INC

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Rifai, Sami
Sent: Sunday, March 24, 2002 8:02 AM
To: [email protected]
Subject: [mems-talk] Etching

Hi all,

I am trying to identify eteching equipment manufacturers. I understand
Alcatel
vacuum is one. Is that right? Who are the other manufacturers?

Thanks

Sami
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing