MEMSnet Home: MEMS-Talk: Helium's role in RIE
Helium's role in RIE
2002-03-28
Peng Yao
2002-03-28
Roger Shile
2002-03-28
[email protected]
2002-03-29
Peng Yao
2002-04-05
Jörn Koblitz
2002-04-08
Michael D Martin
Helium's role in RIE
[email protected]
2002-03-28
Yours is an excellent observation. I have my ideas about what is happening
but I would like to hear what others have observed first especially Bill
Moffett. I find most of his answers to be right on the mark. Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group