MEMSnet Home: MEMS-Talk: radius of curvature measurement
radius of curvature measurement
2002-04-04
David Tang
2002-04-08
Henry Yang
2002-04-09
Roger Shile
radius of curvature measurement
David Tang
2002-04-04
Hello,

I am trying to characterize thin film material properties by measuring the
radius of curvature of specimens that are ~1cmx10cm long.  Does anyone know
of vendors/labs/universities around Boston that have non-contact equipment
to measure radius of curvature?  Thanks.

David Tang
MEMSIC Inc.
100 Burtt Road
Andover, MA 01810
Phone:  978-623-8188 x 237
www.memsic.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing