Bubble free in oxide etching
2002-04-09
fasheng zhou
2002-04-10
Bill Moffat
2002-04-10
Wu-Cheng Kuo
2002-04-11
[email protected]
Bubble free in oxide etching
fasheng zhou
2002-04-09
Dear MEMS friends,

I'm trying to eliminate the bubbles in oxide (PSG)
etching by BOE. But I couldn't find any method up
to now. I will really appreciate it if you can
give me some advice.

Thanks.
Yahoo! Tax Center - online filing with TurboTax
http://taxes.yahoo.com/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing