vacuum oven
2002-04-11
anshu mehta
2002-04-12
Maurice Norcott
vacuum oven
Maurice Norcott
2002-04-12
Blue-M goes up to 260C , I don't think I've seen any go
much higher as the seals won't hold.



-----Original Message-----
From: anshu mehta [mailto:[email protected]]
Sent: Thursday, April 11, 2002 2:02 PM
To: [email protected]
Subject: [mems-talk] vacuum oven


Hi

We are inetrested in buying a vacuum oven which could
to a pressure range of few torr or less and can go up
to temperatures of 400-500C. Also, we want it to have
a mechanical feedthrough to be able to apply pressure
. We want to put a device inside, cover it and seal
using glass frits. the high temperature is required
for firing of glass frits.

Kindly suggest if such oven would be available
off-the-shelf or if we could get it custom made from
somewhere.

Thanks,
Anshu mehta
Yahoo! Tax Center - online filing with TurboTax
http://taxes.yahoo.com/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation