Torsten Gerlach, IMMM, Tel.
High aspect ratio thick photo resist structures
Torsten Gerlach, IMMM, Tel.
1996-08-25
Dear MEMS colleagues,
we are trying to fabricate thick photoresist (30-50um) structures on
silicon substrates.

We are using the resist AR-P 322, lambda 308-450, and developer AR
300-26 from the company Allresist in Berlin, Germany. The exposing is
carried out with an Electronic Vision mask aligner.

The obtained aspect ratio is rather poor. The angle included by the
side-walls and the substrate surface is around 60 deg. No difference
was observed using chromium or photo emulsion masks.

Any suggestions on how to approach the ideal case of vertical side-
walls are apreciated.

Torsten Gerlach

=========================================
Technical University of Ilmenau
Dept. of Micro System Technology
P.O. Box 0565
D-98684 Ilmenau
F.R. Germany
phone: +49 / 3677 / 69-1295,   fax: -1296
=========================================


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing