Jai Shinh
2002-04-15
Mike,
Thank you very much for confirming my observation.
If it is not too much trouble, I wonder if you could
tell me where to find some literature on the
electrochemical effects between Cr/Cu.  I'd appreciate
it a lot.

Best,
Jai

----- Original Message -----
From: "Michael D Martin"

To: 
Sent: Friday, April 12, 2002 8:10 AM
Subject: Re: [mems-talk] Cr/Cu wet etching &
electrochemical reactions?


> There is a strong electrochemical effect between the
two metals. We have
> actually used this effect to selectively protect
chrome in Cr etch. One
> solution may be to bias the chrome, if this is
feasible.
>
> -Mike
Yahoo! Tax Center - online filing with TurboTax
http://taxes.yahoo.com/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
MEMStaff Inc.
MEMS Technology Review