REMOVAL OF NITRIDE
Haigh, Richard
2002-04-22
Dear All

I've had some SOI wafers coated with Si3N4 and patterned on one face.
Unfortunately, the wrong face has been patterned. I don't want to
dispose of the wafers because of their cost. I've been told that I can
have the nitride striped off both faces (with RIE), then re-applied and
patterned on the correct face. What I need to know, does the stripping
damage the silicon in anyway?


Regards



Richard Haigh

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.