MEMSnet Home: MEMS-Talk: PDMS, spin coating
PDMS, spin coating
2002-04-26
RalfAßmann
PDMS, spin coating
RalfAßmann
2002-04-26
Hi everybody!
I want to coat some pmma with pdms by spin coating. Does anyone has some

knowledge about this problem? The thickness must be about 55m. Is there
an ideal viscosity and thinner I can use?
Thanks and best regards!

[demime 0.98e removed an attachment of type text/x-vcard which had a name of
Ralf.Assmann.vcf]