A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Need electroplating equipment
Need electroplating equipment
2002-04-23
Yuqi Jiang
2002-04-28
Igor Kadija
Need electroplating equipment
Igor Kadija
2002-04-28
Hi Yuqi,
if you need electroplating equipment for micro and nano features including
wafer bumping and you need good uniformity, 5% and better, you should look
into www.fibrotools.com. Our standard benchtop electroplating equipment IKo,
30" by 30" footing, is designed especially for lab and clean room
applications for a dependable quick sample turnover and concept testing.

Igor Kadija
ECSI FIBRotools

At 04:04 AM 4/23/02 -0700, you wrote:
>Dear everone,
>   I'm seeking for the electroplating equipment for
>wafer bumping. This equipment should be appropriate
>for experiments in lab.
>   If anyone provides the websites or companis'
>names,I will be very grateful.
>
>   Yuqi
>Yahoo! Games - play chess, backgammon, pool and more
>http://games.yahoo.com/
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Mentor Graphics Corporation
Harrick Plasma, Inc.