MEMSnet Home: MEMS-Talk: start point of bosch
start point of bosch
2002-04-29
Peng Yao
2002-04-29
___
2002-04-29
[email protected]
start point of bosch
[email protected]
2002-04-29
Unless your rie system is equipped with a helium backside cooling capability,
a high density source for disassociation of the proper gases, a turbo pump,
and bias capability on the wafer chuck you might be disappointed in the
profile. Bob Henderson