A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: photoimageable insulator
photoimageable insulator
2002-05-03
Martin O. Patton
2002-05-07
shay kaplan
2002-05-07
___
2002-05-08
carlton watson
2002-05-06
Bill Moffat
2002-05-08
Greg Miller
2002-05-09
carlton watson
photoimageable insulator
Bill Moffat
2002-05-06
Martin,
        photoimageable Polymide or B.C.B. sounds like the answer.  Bill Moffat

-----Original Message-----
From: Martin O. Patton [mailto:[email protected]]
Sent: Friday, May 03, 2002 11:14 AM
To: [email protected]
Subject: [mems-talk] photoimageable insulator


Dear mems-talkers,

Is there a photoimageable insulator that can be applied to insulate trenches
in III-V wafers from metal contacts which cross the trenches?  I only have
wet chemistry, so don't tell me to RIE.

Thanks,

Marty

Martin O. Patton
Senior Research Engineer
Essential Research Inc.
6410 Eastland Road Suite D
Cleveland, Ohio 44142
www.er.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMS Technology Review