Shadow masks
___
2002-05-10
 Stephen,
Can you provide more details as to the pattern and aspect ratios involved?  Have
you considered using Silicon?  How about Fotofab?  I've never used them, but it
looks like they can do about 1/2 mil over 6":
http://www.fotofab.com/Design_Considerations/Tolerances/tolerances.html
Neal

  Stephen Bart  wrote: I am looking for vendors who
can construct a 6 in shadow mask with 1 mil
(25um) or better
resolution.

Any suggestions?

--
*******************************************************************

Stephen F. Bart, Ph.D.

Technical Fellow, Core Technology Development

Coventor, Inc.
625 Mount Auburn Street
Cambridge, MA 02138 USA

*******************************************************************
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
Yahoo! Shopping - Mother's Day is May 12th!

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics