MEMSnet Home: MEMS-Talk: Multilayered SU-2075 structures
Multilayered SU-2075 structures
2002-05-10
Kris Armoogum
2002-05-12
Yohannes M Desta
Multilayered SU-2075 structures
Yohannes M Desta
2002-05-12
Kris,

We have achieved multi-layer microstructures by using
ebeam evaporated metal between the various photoresist
layers to protect the underlying resist layer from
exposure. Give it a try.

Good luck,

Yohannes

--- Kris Armoogum  wrote:
> Dear All,
>
> Has anyone attempted to create a two layered
> structure using Su-
> 2075 where the top layer OVERHANGS the bottom layer?
>
> I am trying to do this using conventional
> photolithography methods
> but without success.
>
> Because the Su-2075 is so transparent, it is
> difficult to judge the
> exact exposure time so that the top layer is not
> crosslinked all the
> way down to the wafer surface.
>
> A sales rep from one of the Su-2075 manufacturers
> thinks this is
> impossible.
>
> Best regards.
>
>
>
>
>
>
> Kris Armoogum
> Microengineering & Biomaterials Group
> Dundee University Tissue Engineering Centre
> School of Engineering,
> University of Dundee
> Dundee DD1 4HN
> Tel: 0044 1382 345641
> Email: [email protected]
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.mems-exchange.org/
LAUNCH - Your Yahoo! Music Experience
http://launch.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.