Help on thick photoresist
2002-05-15
hongyuyu
2002-05-17
Robert Okojie
2002-05-16
Michael D Martin
2002-05-16
[email protected]
2002-05-16
Danny Hirdes
2002-05-17
Bill Moffat
Help on thick photoresist
[email protected]
2002-05-16
> In bulk microfabrication, I tried to fill a deep channel,
> which is around
> 200um. When I use AZ5214, there are lots of air bubbles
> coming out when I
> bake it. So how can I solve this problem?
> Do I need to use different PR? High thick PR?
> I want to try SU-8, but my friends told me that is a dirty
> material and
> not easy to remove after baking.

Try spraying acetone on the wafer before spinning.
While the wafer is still wet, dispense the resist and spin.
The acetone aid in wetting, and may work for you
depending on your exact geometry
        --Kirt Williams Agilent Technologies

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.