Highest resistivity silicon?
2002-05-20
Fred Hussain
2002-05-20
Michael Pedersen
2002-05-20
David Nemeth
2002-05-20
Michael Barger
2002-05-20
Kenneth Smith
2002-05-22
mmf
2002-05-20
Kenneth Smith
2002-05-20
Michael D Martin
Highest resistivity silicon?
Kenneth Smith
2002-05-20
Final note here- Westinghouse does not produce FZ Silicon anymore either
since early 90s. So likely it is >15,000 or more like >12,000 ohm-cm
unless you want just a few slices then there are likely some from first
2 cm of the growth >20,000 ohm-cm if luckily.
Good luck in the search and should you find a source let us know.

Regards,
Ken

Michael Bragger wrote:

> Fred,
>
> I guess I need to weigh in here. The intrinsic resistivity of silicon is 240
> kOhm-cm as indicated on the tydex web site. This is the theoretical limit.
> It also mentions that 30 kOhm-cm is available. Generally, this is about the
> best you are going to get. Anything that you do to this material will reduce
> the resistivity, period. The degree to which you are careful will determine
> how much the resistivity will be reduced. The highest resistivity material
> that I have ever seen was 100 kOhm-cm, which was probably close to a world
> record. I was able to get a 3-inch diameter boule of this material from
> Westinghouse in the early 90's. Unfortunately, they did not and do not sell
> silicon commercially and my contacts are no longer there.
>
> Good luck,
>
> Mike Barger
> Klesis Corporation
>
>
> -----Original Message-----
> From: [email protected] [mailto:[email protected]]On
> Behalf Of David Nemeth
> Sent: Monday, May 20, 2002 11:44 AM
> To: [email protected]
> Subject: RE: [mems-talk] Highest resistivity silicon?
>
>
> First, 250 K-Ohm cm seems like an unrealistically high value.  I've seen
> silicon up to 12 KOhm-cm, and have used material up to 6KOhm-cm.  Looking at
> the web site, they don't actually seem to produce this value - it might just
> be the theoretical resistivity of pure silicon with no dopants that they are
> quoting.
>
> There are other suppliers of high-resistivity silicon, for example wacker
> and topsil.
>
> Next, I've heard (but can't say for sure) that if you grow a thermal oxide,
> the resistivity will never be higher than a few thousand ohm-cm when your
> done, no matter how good it was to start.  Any thermal treatment will
> diffuse some impurities into the wafer, depending on the time and
> temperature of the treatment.
>
> If you need to end up with 2000 ohm-cm, your probably fine.  If you need to
> end up with 6000 ohm-cm, you will need to be careful about your thermal
> processing and may have problems.  If you need 250000 ohm-cm, your probably
> out of luck.
>
>
> David Nemeth
> Senior Process Engineer
> Sophia Wireless, Inc.
> 14225-C Sullyfield Circle
> Chantilly, VA
> Ph: (703) 961-9573 x206
> Fax:(703) 961-9576
>
> -----Original Message-----
> From: [email protected] [mailto:[email protected]]On
> Behalf Of Fred Hussain
> Sent: Monday, May 20, 2002 6:47 AM
> To: [email protected]
> Subject: [mems-talk] Highest resistivity silicon?
>
>
> Dear all,
>
> I am looking for silicon substrates which can be machined using conventional
> MEMS type processes, but at the same time are highly insulating. I've found
> a web page with silicon of 250Kohm-cm resistivity -
> http://www.tydex.ru/materials/materials2/Si.html.
>
> Does anybody:
> have any experience of working with such materials?
> know of any issues, for example the stability of the resistivity with
> temperature?
> micromachined it without any major issues?
> know of any suppliers?
>
> Thanking you in advance.
>
> Regards,
>
> Fred.
>
> --------------------------------------------
> Dr Fred Hussain
> The Technology Partnership plc
> Melbourn Science Park
> Cambridge Road
> Melbourn
> Royston
> Hertfordshire
> SG8 6EE
>
> Tel: 01763 262626
> Fax: 01763 261582
> www.ttpgroup.com
> ---------------------------------------------
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
>
>


--


Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG, SOS.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
The Branford Group
Nano-Master, Inc.