MEMSnet Home: MEMS-Talk: Gold film
Gold film
how to deposit PZT
2002-05-10
Haigh, Richard
how to deposit PZT
2002-05-10
RobDavis
2002-05-13
Gurvinderjit Singh
2002-05-14
Christopher F. Blanford
tin on copper oxide
2002-05-14
Robert Dean
PLZT robotics
2002-05-22
Gurvinderjit Singh
how to deposit PZT
2002-05-10
Michael Barger
how to deposit PZT
2002-05-10
lucp1429
how to deposit PZT
2002-05-12
TEL Klaus Beschorner
how to deposit PZT
2002-05-13
Haigh, Richard
2002-05-20
Gurvinderjit Singh
2002-05-20
___
2002-05-21
Ravi Shankar
2002-05-21
Michael D Martin
2002-05-22
Henry Yang
2002-05-25
TEL Klaus Beschorner
Gold film
Henry Yang
2002-05-22
What is the condition of your annealing chamber?

Henry

--------------------------------------------------------------
Henry Yang
Mechanics and Micromechanics Group
IBM Almaden Research Center
408-927-2319



                      Ravi Shankar
                                          cc:
                      Sent by:                 Subject:  Re: [mems-talk] Gold
film
                      mems-talk-admin@m
                      emsnet.org


                      05/21/2002 09:43
                      AM
                      Please respond to
                      mems-talk





what is the conditions in your evaporation system.
Ravi shankar


On Mon, 20 May 2002, Gurvinderjit Singh wrote:

> Dear friend i have one query.
> I am depositing gold film (thickness 0.1 micron)by thermal evaporation on
> oxides,
> but when  i am annealing my sample to 700K this gold film become non
> -conductive may be  duo to formation of gold oxide. But from
> literature i found
> that gold should not become oxide till 1200K. I also read people using
> gold electrodes (thin film by thermal evaporation) on their samples and
> work till 900k kindly let me know where i am doing mistake, wether to
take
> more thick film or something else.
>
>
>
>
_______________________________________________________________________________

>
>
>    Gurvinderjit Singh Ahluwalia             Tel: +91-0731-488656
>      Laser Materials Division               Fax: +91-0731-488650
>    Centre for Advanced Technology         email: [email protected]
>    Indore - 452 013  INDIA
>
>
_______________________________________________________________________________

> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Nano-Master, Inc.
MEMStaff Inc.