3. dielectric materials can survive HF
Andrea Leppart
2002-05-31
Silicon carbide is untouched by HF and has a dielectric constant of 9.7
(comparable to silicon, more than double that of oxide or nitride).  Please
contact me off-list if you would like to have your chips coated.

Regards,

Andrea Leppart

____________________________

Andrea Leppart
VP, Business Development
FiberLead, Inc.
[email protected]
Tel:  917-693-1937
Fax: 212-608-6840


----------------------------------------------------------------------------
CONFIDENTIALITY NOTICE: This message is intended only for the use of the
individual or entity to which it is addressed and may contain information
that is privileged, confidential or exempt from disclosure under applicable
law.  If the reader of this message is not the intended recipient (or a
person authorized to deliver it to the named addressee), you are hereby
notified that you are strictly prohibited from printing, storing,
disseminating, distributing or copying this communication.  If you have
received this communication in error, please notify the sender immediately
by replying to the message and deleting it from your computer. Thank You.
----------------------------------------------------------------------------

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Harrick Plasma, Inc.
MEMS Technology Review