Martin HEDSTROM
2002-06-05
Shahram Malek
2002-06-05
Bill Moffat
2002-06-05
Bill Moffat
2002-06-07
Michael D Martin
Polyimide residue removal
Shahram Malek
2002-06-05
Hi Martin,

You can use a UV-Ozone Cleaning process to remove the remaining 100-500 nm
of polyimide. Please visit our Web site at
http://www.samcointl.com/prod/UVO.html for our line of UV-Ozone Cleaners
and contact me if you have any questions or would like to receive
additional information. I look forward to helping you with your
application.

Shahram



Martin HEDSTROM wrote:

> Hi all,
>
> I have a problem with removal of polyimide residues under a nitride
> membrane. The polyimide is removed in a pure O2-plasma since I am afraid
> that any CF4 addition might hurt the nitride membrane. Apparently this
> O2-plasma is not sufficient since I get small residues left with about
> 100-500 nm thickness.
>
> Does anybody know about any dry etchant which can remove the last of the
> polyimide without damaging the nitride membrane?
>
> Thanks in advance
>
> /Martin
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review