MEMSnet Home: MEMS-Talk: tweezer for coated film handling?
tweezer for coated film handling?
2002-06-03
jingliu
2002-06-05
Kenneth Smith
2002-06-06
Christopher F. Blanford
tweezer for coated film handling?
Christopher F. Blanford
2002-06-06
For handling coated surfaces here, we either use spatula-ended tweezers
wrapped with PTFE pipe tape or PTFE-coated metal tweezers. From Fisher,
the former cost about #2 and the latter costs around #11. Ten meters of
PTFE tape cost about #11. A "poor-man's" solution, but it does the job.

Regards,

Chris

jingliu wrote:

> To who may concern,
> I got metal (Au) coated on my small samples ( a few mm ). I need to find
> some tweezers to handle the sample without damaging the coated surfaces
> during handling and transfer.
> I've heard that there are some rubber tweezers? Can it withstand 100
> Celsius? Could anybody suggest me the vendor information?
> Thanks,
> Jing

--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: (44)/(0)-1865-282603; Fax: (44)/(0)-1865-272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review