MEMSnet Home: MEMS-Talk: Help on high aspect ration Polyimide RIE
Help on high aspect ration Polyimide RIE
2002-06-10
Bo-Kuai Lai
2002-06-10
[email protected]
Help on high aspect ration Polyimide RIE
Bo-Kuai Lai
2002-06-10
Dear all:

I am looking for the foundary which can do RIE of polyimide.

The polyimide is PI2611, not photo definable, which is 10 um thick and the
patterns were already defined by Al layer.

The side wall of polyimde needs to be close to vertical.

Thanks




Bo-Kuai Lai
Departmet of Materials Science nd Engineering
Case Western Reserve University
10900 Euclid Ave.
Cleveland, Ohio 44106
Phone: 216-368-4819
Fax:   216-368-4209
Sign-up for Video Highlights of 2002 FIFA World Cup

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer
The Branford Group