Dear Mems specialists,

I am searching for a way to deposit a high reflective coating inside small
holes in PC.
These holes are about 10um radius and 100um deep.
Any suggestions about the technology to use?
Could Al sputtering give a good coverage and what is the reflection% could
we expect?

Any help is highly appreciated.

Thanks,

Martin De Kegelaer

***************************************************************
Martin De Kegelaer
Agfa-Gevaert N.V.
Research Center on Electronic Imaging
Septestraat 27,
2640 Mortsel
Belgium
tel: +32 3444 6243
fax: +32 3444 6450
***************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.