Hi Masahiro Tsugai,

I went through your question on mems-talk sent by you today.
According to the handbook I have on "LSI process technology",
the thermal expansion coefficient of TiN is 6.3x10-6 @20degC.
I am sure this value is trustworthy.

Tsukasa

----- Original Message -----
From: "Masahiro Tsugai" 
To: 
Sent: Wednesday, June 12, 2002 5:23 PM
Subject: [mems-talk] TiN


> Dear friends,
>
> I would like to get information regading tecnical papers
> dealing with thermal expantion coefficient of TiN thin layer.
>
> Thanks in advance.
> Masahiro
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review