Thick insulator layer(~6 um) SOI wafer
2002-06-11
[email protected]
2002-06-19
Soojin Oh
2002-06-21
Kenneth Smith
Thick insulator layer(~6 um) SOI wafer
Soojin Oh
2002-06-19
I am not sure if you still need this information. I
could buy 4 micron thermal oxide wafers from this
company. (www.universitywafer.com) I recall they even
had 10 micron thick oxide wafers. But know the price
is outrageous.
Best regards.
Sue

--- [email protected] wrote:
> Hello!
>
>   We are trying to find SOI wafer with thick SiO2
> layer about 6um thickness.
>
> Or If you know some group or person who deposite
> SiO2 film more than 6 um. Please,
>
> Let me know the contact point.
>
>   We are looking for sacrificial layer for
> poly-silicon actuator structure.
>
>
> Have a nice day for everybody.
>
>
>
> ----------------------------------
> Soon Cheol Kweon
>
> Members of Technical Staff.
> MEMS Lab.
>
> SAMSUNG
> Advanced Institute of Technology
>
> P.O.Box 111, Suwon
> 440-600, KOREA
>
> TEL:82-31-280-9448
> Fax:82-31-280-9473
> E-mail:[email protected]
>         [email protected]
> -------------------------------------
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/
Yahoo! - Official partner of 2002 FIFA World Cup
http://fifaworldcup.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
MEMStaff Inc.