MEMSnet Home: MEMS-Talk: Thermal growth rates of Aluminum Oxide
Thermal growth rates of Aluminum Oxide
2002-06-18
Nicholas Jankowski
2002-06-18
RobDavis
2002-06-19
Nicholas Jankowski
2002-06-19
Michael D Martin
2002-06-21
Nicholas Jankowski
2002-06-19
BERAUER,FRANK (HP-Singapore,ex7)
2002-06-21
Nicholas Jankowski
2002-06-22
[email protected]
2002-06-22
Nicholas Jankowski
2002-06-24
Dave Howorth
Thermal growth rates of Aluminum Oxide
Nicholas Jankowski
2002-06-21
"BERAUER,FRANK (HP-Singapore,ex7)" wrote:
>
> Just a thought: Why don't you just deposit more Al, such
> that after the erosion you have the thickness you desire?
> You said "not negotiable", but certainly sputtering a bit
> longer is something every Fab can do.

it would if i sputtered it on in the first place :)  See my previous
message to the list...

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering