A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Stability of SU-8 in metal etchant?
Stability of SU-8 in metal etchant?
2002-06-23
Tao Xu
2002-06-24
BERAUER,FRANK (HP-Singapore,ex7)
Stability of SU-8 in metal etchant?
Tao Xu
2002-06-23
Hi, Everyone,

    we have a problem in making SU-8 suspension structures, such as cantilever
or bridge structure. We used Cu or Ni as the sacrificial layer. After we etched
the Cu or Ni to release the suspension structure, the SU-8 cantilever or bridge
was bended and misalignment. We cannot get the straight cantilever. Do you think
that was because of the SU-8 stress issue, or because the metal etchant attacked
the SU-8 and made it soft. Could you give us some suggestions about that?

Thanks,

Tao

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer