Hi,  I have a problem with removing fluorocarbon reside off a deep silicon
trench sidewall after a DRIE process (SF6, C4F8 gases used).  Lot of papers
suggest that the polymer can be removed by O2 plasma, but it seems like the
polymer on my wafer get hardened by oxygen plasma.

If you know why sidewall polymer can harden(?) or know how to remove a such
tough polymer, please email to me at [email protected]

Thank you

Ken

_________________________________________________________________
Chat with friends online, try MSN Messenger: http://messenger.msn.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
University Wafer