I have always developed PMMA with a mixture of MIBK and IPA -
this web page should help with the mixtures:
http://www.microchem.com/products/pdf/PMMA_Data_Sheet.pdf

Hope this helps,

Greg Miller
KVH Industries
Email: [email protected]


-----Original Message-----
From: Haigh, Richard [mailto:[email protected]]
Sent: Wednesday, June 26, 2002 3:31 AM
To: [email protected]
Subject: [mems-talk] RE: PMMA developers


Hi

I am interested in solvents that can be used for the development of
polymethylmethacrlate photo-resists. Does anyone know of a company that
supplies these. I have an application that requires unhydrous solvents.

Richard Haigh
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.
University Wafer