MEMSnet Home: MEMS-Talk: Deep trenches filling
Deep trenches filling
2002-06-26
qwer 1234
2002-06-26
Greg Mattiussi
2002-06-27
qwer 1234
Deep trenches filling
Greg Mattiussi
2002-06-26
> We need to fill deep trenches (1*10um) etched in the silicon layer of
SOI
> wafer with a material that has a refraction index close to but
different
> from that of Si (3.5).


You might want to try polysilicon.  It has excellent step coverage
(LPCVD or RTCVD) and has an index close to but not equal to that of
crystalline silicon (see "Optical study of undoped, B or P-doped
polysilicon", Y. Lahla and E. Scheid, Thin Solid Films 306 (1997) pp.
67-73).  RTCVD can generally fill trenches more completely than LPCVD
since the dep rate is higher and the films are smoother.

Cheers,

Greg Mattiussi
Spectalis Corp.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.
The Branford Group