A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: shear modulus of nickel
shear modulus of nickel
2002-06-25
Di Chen
2002-06-26
Christopher F. Blanford
shear modulus of nickel
Christopher F. Blanford
2002-06-26
Dear Dr Di Chen

Efuna (http://www.efunda.com/) lists a value of 80 GPa.

Chris

On Wednesday, June 26, 2002, at 04:12  am, Di Chen wrote:

> Dear MEMS colleagues,
> Anyone can kindly help me to find the shear modulus of nickel?
>  Thanks a lot
>
> Prof. Di Chen
>
> Shanghai Jiao Tong University
>
> [email protected]

--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: (44)/(0)-1865-282603; Fax: (44)/(0)-1865-272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review