RE: shear modulus of nickel
2002-06-27
Yanjun(David) Tang
RE: shear modulus of nickel
Yanjun(David) Tang
2002-06-27
 Dear Prof. Di Chen:
 I think you can check Ni shear modulus in the following website, which is
 80MPa.

http://www.efunda.com/materials/common_matl/Common_Matl.cfm?MatlPhase=Solid&
MatlProp=Mechanical#Mechanical

 Best regards

 Yanjun(David) Tang

 Graduate student
 Institute for Micromanufacturing
 Louisiana Tech University

 1401 Tech Farm Rd. Apt. #238, Ruston, LA 71270, USA
 Email: [email protected]
           [email protected]
 Homepage: http://www.latech.edu/~yta001/index.htm
 Tel: 1-318-255-5133

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing