Hello,
I  am looking for information about chrome etchant with a very slow etch
rate  about  5 A per second or slower,
Currently I work with Chrometch 3144 produced by Alliedsignal - but this
product is too strong ~ 33 A per second (maybe someone know  how dilute
this)
Thanks in advance
Lukas

--
****************************************
Lukasz Nieradko, Ph D

Laboratoire d'Optique P.M. Duffieux,
Faculte des Sciences et Techniques
16 route de Gray, 25030 Besancon, France

tel: +33-381-666-410, fax: +33-381-666-423
email: [email protected]
****************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
MEMStaff Inc.
Tanner EDA by Mentor Graphics