MEMSnet Home: MEMS-Talk: biocompatibility coating on Nickel probes
biocompatibility coating on Nickel probes
2002-07-03
gang hong
2002-07-08
Mike Mattes
biocompatibility coating on Nickel probes
Mike Mattes
2002-07-08
Tinghui,

I would recommend gold. You also might want to use an adhesion/ barrier metal
underneath the gold, such as titanium. Make sure the oxide on the nickel has
been removed before depositing your biocompatible metals. If you intend to
make connections to the microprobes with wires you have another problem area.
How will you make these connections? Solder is not biocompatible. Perhaps a
final gold layer can be electroless plated on the microprobes and connections.
Take care not to use cyanide based electroless gold.

Regards,
Mike Mattes
Medtronic, Inc.

>>> [email protected] 07/03/02 09:28AM >>>
Hi folks,

I am fabricating Nickel Microprobes which are used in
medical applicatioins. Therefore I need to consider
the biocompatibility with human tissue. What
coating(s) should I apply on the probes and how? Can
somebody give some suggestions?

With a lot of thanks!

Tinghui
RxPP>^M7>[;aVPT- 4s@KLT!.=p!/K-=+P&0A
http://sweepstakes.yahoo.com/bank_surveywave2/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.