About the Photosensitive glass
2002-07-16
Peng Jin
2002-07-16
Fred Hussain
About the Photosensitive glass
Fred Hussain
2002-07-16
Peng,

If you're after photostructurable glass, you can use FOTURAN from
Mikroglass:

http://www.mikroglas.com

Regards,

Fred.

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Peng Jin
Sent: 16 July 2002 12:59
To: [email protected]
Subject: [mems-talk] About the Photosensitive glass


Dear fellow MEMS Researchers,

In my experiment, I plan to use the photosensitive glass for high aspect
ratio
structure. I remember that there were some informtion about it. But I can
not
find it now.

Could you provide some information about the supplier of this kind of thing.
If there are somebody has done this before, could you tell which kind
equipment is necessary for it?

Any suggestion are highly appreciated.

Cheers

Peng
>=========================================
>Dr. P. Jin
>Research Associate
>School of Manufacturing and Mechanical Engineering
>The University of Birmingham
>Edgbaston, Birmingham B15 2TT
>Tel:  ++44-121-414-4256
>=========================================
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
The Branford Group
Process Variations in Microsystems Manufacturing