contact angle
2002-07-16
changhong ke
2002-07-17
Xiaodong Yan
2002-07-17
Stephen P
2002-07-16
HUANG Xudong
2002-07-17
Michael D Martin
2002-07-18
CLIF HAMEL
2002-07-18
Xiaodong Yan
2002-07-19
[email protected]
contact angle
HUANG Xudong
2002-07-16
I measured the static contact angle for water on Si substrate (with native
oxide) very recently, it is around 21 degree.

regards,

xd

-----Original Message-----
From: changhong ke [mailto:[email protected]]
Sent: Wednesday, July 17, 2002 2:51 AM
To: [email protected]
Subject: [mems-talk] contact angle


Dear Members:

Currently I want to know the contact angle of water on Si substrate and Cr
substrate. However, I couldn't find it in  handbooks.
If you happen to know the information, please drop me an emai, your help is
greatly appreciated.

changhong
--------------------------------------
Changhong Ke
Mechanical Engineering
Northwestern University
2145 Sheridan Road
Evanston,IL 60208-3111 USA
Lab Phone:(847)467-7673
Fax:(847)491-3540
E_mail:[email protected]
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing