Gold etching
2002-07-19
Luciano Scaltrito
2002-07-19
Roger Shile
2002-07-19
David Nemeth
2002-07-19
Martin, Dick
Gold etching
David Nemeth
2002-07-19
However, I've found that iodine based etches will aggressively undercut
Nickel if there is gold on top of it.  It's pretty weird.

Some sort of physical process (RIE using Argon or ion mill) would probably
be the best, if you have access to it.

David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Roger Shile
Sent: Friday, July 19, 2002 2:20 PM
To: '[email protected]'
Subject: RE: [mems-talk] Gold etching


Transene TFA Gold Etch, which is an aquous solution of iodine and potassium
iodide, will etch the gold in a few seconds.

-----Original Message-----
From: Luciano Scaltrito [mailto:[email protected]]
Sent: Friday, July 19, 2002 1:24 AM
To: [email protected]
Subject: [mems-talk] Gold etching


Dear colleagues,

>I have a problem. I have to etch a thin film (200 angstrom) of Gold over a
>film of Nickel but I DON'T have to remove Nickel.

How can I do this?

Thank you
Luciano Scaltrito

----------------------------------------------------------------------------
------------
                ~ The truth is out there ~
Ing. Luciano Scaltrito
Dipartimento di Fisica
Politecnico di Torino
C.so Duca degli Abruzzi, 24
10129 Torino, Italy
tel +39 011 564.7305/564.4160
fax +39 011 564.7399
E-mail : [email protected]
http://www.polito.it/centri/laborato/limadel/film/index.html
----------------------------------------------------------------------------
-----------
-
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
"This email and any attachments may contain information that is confidential
and proprietary information of Veeco Instruments Inc. and are intended only
for the use of the addressee. Unauthorized use, distribution or copying is
forbidden. If you have received this email in error, please notify the
sender immediately by return email and delete all copies of this message and
any attachments from your computer. Thank you."
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing