MEMSnet Home: MEMS-Talk: adhesion of Ag to Si
adhesion of Ag to Si
2002-07-24
Thomas B. Jones
2002-07-25
Jeff Zahn
2002-07-26
Zhen YANG
2002-07-24
[email protected]
2002-08-14
TEL Klaus Beschorner
adhesion of Ag to Si
Zhen YANG
2002-07-26
I use Ag/Au/Cr in my electrode for dissolved oxygen detection. It works
well.

__________________________

            Zhen  YANG,  Ph.D.
            Institute of Mechanical System Engineering
            AIST
            Namiki 1-2,  Tsukuba
            JAPAN  305-8564

----- Original Message -----
> ..... Will a thin layer of Cr help to improve this adhesion?
> Finally, are there other straightforward methods to promote adhesion of
> these materials?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.