Adhesion of metal to epoxy substrates
2002-08-07
Fred Hussain
2002-08-07
Greg Miller
2002-08-07
Bill Moffat
2002-08-09
Fred Hussain
2002-08-09
Bill Moffat
Adhesion of metal to epoxy substrates
Bill Moffat
2002-08-07
Fred,
     This could explain a number of special units we have built with no
indication of the final use.  These are special Plasma/Silane deposition
units.  Think stainless oven set at 150 degrees C able to do vacuum priming
with flat capacitive stainless plasma generators for precleaning.  let me know
if you want to test this approach.  Bill Moffat

-----Original Message-----
From: Fred Hussain [mailto:[email protected]]
Sent: Wednesday, August 07, 2002 1:31 AM
To: [email protected]
Subject: [mems-talk] Adhesion of metal to epoxy substrates


Dear Collegues,

I am looking for any advice/information on how to improve adhesion of
evaporated metal (nichrome + gold) onto thermo-epoxy based substrates. In
particular, information on chemical and physical (plasma) surface
pre-treatments and/or alternative metals which may have a distinct advantage
over nichrome and gold, would be highly appreciated.

Thanking you in advance,

Fred.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Addison Engineering
Tanner EDA by Mentor Graphics