MEMSnet Home: MEMS-Talk: Contamination issue of additive in THAH etching
Contamination issue of additive in THAH etching
2002-08-12
[email protected]
2002-08-12
Tabada, Phillipe
2002-08-13
Michael D Martin
Contamination issue of additive in THAH etching
[email protected]
2002-08-12
Hi all,
i am working on silicon anisotropic etching using TMAH recently,
in order to control the roughness of etched silicon and the selectivity to
Al and oxide,
we add silicic acid (SA) and ammonium persulfate (AP),
and as refer to S. Brida's recipe,
we add 2.5g AP per 15min to the etchant (~2L) to maintain the etching rate,
after 1~3 hours of etching,
we take the sample out the etchant,
and rinse it in DI water,
and there are plenty of contamination over the sample,
if anyone have any ideal or experience about how to avoid the contamination
issue,
many thanks,

Reference paper : S. Brida,"Microstructures etched in doped TMAH
solutions," Microelectronic Engineering, 53 (2000), 547-551

Grace Kuo
====================================
Global Communication Technology, Corp.
8F, No. 10, Prosperity Rd. 1 , SBIP,
Hsin Chu, Taiwan, R.O.C.
Tel : 886-3-5638686 ext . 7201
Fax : 886-3-5638432
E-Mail : mailto:[email protected]
====================================

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Nano-Master, Inc.
Harrick Plasma, Inc.